Electric Melting And Boosting For Glass Quality Improvement

Each year, new electric boost systems are incorporated into new fuel or oxy-fuel-fired furnaces, and a much greater number of boost systems are added, reinstalled or enlarged in the course of furnace repairs. In many of these cases the boost system is still seen primarily as a means of increasing furnace output, to be used only when necessary. But this underestimates the potential of electric boosting to influence overall furnace operation, energy consumption and glass quality, as well as just adding energy to the melting process and increasing output. In the first part of this article, the author looks at how electric boosting can help improve the quality of glass being produced.

Author
Un-named
Origin
Unknown
Journal Title
Glass Worldwide Sept-Oct/2009 38-41
Sector
General
Class
G 3669

Request article (free for British Glass members)

Electric Melting And Boosting For Glass Quality Improvement
Glass Worldwide Sept-Oct/2009 38-41
G 3669
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.