Electric Furnaces And Systems For Batch Charging

In this article, the author discusses batch charging in relation to the successful operation of all-electric glass melting furnaces, drawing on function, requirements, distribution needs and type.

Author
R Sims
Origin
Nikolaus Sorg Gmbh, Germany
Journal Title
Glass International Feb/09 38-40
Sector
General
Class
G 3609