Electric Furnace Application For Container Glass

An all-electric furnace was commissioned to melt 162 tonnes/day and during 3 years operation melted UVA green, flint and emerald green glasses. The history of the campaign is described.

Author
R D Moore, R E Davis
Origin
Gallo Glass Co, Toledo Engineering Co, Inc
Journal Title
Ceramic Engng Sci Proc 1987 8 3-4 188-199