Elastic Properties And Molar Volume Of Rare-Earth Aluminosilicate Glasses

The elastic properties, molar volume and glass transition temperature of rare-earth-containing aluminosilicate glasses are investigated in the compositions of SiO2-LnAlO3 and SiO2-Ln(3/4)Al(5/4)O3, where Ln is Y, La, Nd, Eu or Yb.