Efficient Crown Insulation

Bulgarian Lubisol Engineering has manufactured a new generation of very light and efficient crown insulating monolithic materials. One of these, Lubisol 2-SL, has a specific density of only 0.33kg/dm3, working temperature of 1,400 deg C, and thermal conductivity of only 0.08 W/mK. According to Lubisol, the high insulating ability of this material reduces the needed thickness of the insulation. One layer of Lubisol 2-SL has the thermal efficiency of two layers of brick insulation with a better thermal efficiency at a lower cost. For more information please see: www.lubisol.ttm.bg