Efficiency Of Luminescence In Luminescent Solar Concentrators

The power efficiency of luminescence excited by solar radiation in luminescent solar collectors is calculated for a glass sheet doped with Cr3+. The achievable chemical potential for an optically thick absorber irradiated by diluted blackbody radiation as a function of Cr3+ concentration, sheet thickness, sunlight dilution, and luminescence quantum yield leads directly to overall conversion efficiency of solar power to luminescence power.

Author
A Lempicki
Origin
Unknown
Journal Title
Applied Optics 22 8 1983 1160-1164 Dx.Doi.org/10.1364/Ao.22.001160
Sector
Special Glass
Class
S 3815

Request article (free for British Glass members)

Efficiency Of Luminescence In Luminescent Solar Concentrators
Applied Optics 22 8 1983 1160-1164 Dx.Doi.org/10.1364/Ao.22.001160
S 3815
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.