Effects Of The Rare Earth Modifier On The Brillouin Scattering From Soda Magnesia Alumina Silicate Glasses

Brillouin scattering spectra of rare earth doped glasses have been measured to investigate the differences of optical properties of soda magnesia alumina silicate glasses with different Eu3+ and Pr3+ concentrations.