Effects Of Radiation On The Properties Of Infrared Fused Silica

Radiation effects of high-energy electrons and protons on properties, optical surface figure of infrared fused silica were studied. Radiation effects of high-energy electrons on surface figure of infrared fused silica were investigated. The results show that mirror surface deformations are not obvious. Radiation effects of protons of surface deformation, visible and infrared reflectances were investigated. The results suggest that radiation effects of high-energy protons on surface deformation and reflectances had not been observed.

Author
Q. Yafan & F Jingzhong
Origin
Chinese Academy Of Sciences, Chengdu, China
Journal Title
Proc 17Th Int Cong Glass, Beijing Vol 3 October 1995 338-343
Sector
Special Glass
Class
S 1287

Request article (free for British Glass members)

Effects Of Radiation On The Properties Of Infrared Fused Silica
Proc 17Th Int Cong Glass, Beijing Vol 3 October 1995 338-343
S 1287
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.