Effects Of Pb On Thermal Stability And Crystallization Kinetics Of Ges2-Sb2S3-Pbs Glasses

Effects of Pb on thermal stability and crystallization kinetics of chalcogenide glasses have been carried out by a detailed calorimetric study and structural analysis. The glass stability was assessed based on three criteria, while the activation energies of crystallization were calculated under non-isothermal crystallization conditions by the Kissinger method, the Augis/Bennet method, the Mahadevan method and the modified Ozawa method, respectively. Both stability criteria and activation energies of crystallization suggest that the glasses possess excellent thermal stability.

Author
G Yang Et Al
Origin
Shanghai University, China
Journal Title
Int J Appl Glass Sci 7 3 Sept/2016 337-344
Sector
Special Glass
Class
S 4283

Request article (free for British Glass members)

Effects Of Pb On Thermal Stability And Crystallization Kinetics Of Ges2-Sb2S3-Pbs Glasses
Int J Appl Glass Sci 7 3 Sept/2016 337-344
S 4283
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.