The Effects Of Particle Size And Additions Of Na2So4 And Nano3 On The Reactions In Soda-Lime-Silica Glass Batches

The coupled effects of particle size and additions of 1 wt% Na2SO4 or NaNO3 on the melting reactions in a multicomponent system were studied using data from thermal analysis and x-ray diffraction interactively.