Effects Of Forming Conditions On Glass Fibre Structures And Properties

This paper reviews recent work on the effect of forming conditions on glass structure and properties. Both silicate and chalcogenide glasses are shown to be strongly influenced by forming, particularly when the conditions approach those associated with "shear thinning". Distinct relaxation peaks, superimposed on a broad sub-Tg exotherm, are observed in Differential Scanning Calorimetry (DSC) of commercial silicate and As2Se3 fibres.

Author
W C Lacourse Et Al
Origin
Alfred University, Usa
Journal Title
Glastech Ber Glass Sci Technol 68 C2 1995 4-13
Sector
Glass Fibre
Class
GF 148

Request article (free for British Glass members)

Effects Of Forming Conditions On Glass Fibre Structures And Properties
Glastech Ber Glass Sci Technol 68 C2 1995 4-13
GF 148
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 17 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.