Effects Of Direct Current On Molybdenum Boosting Electrodes

In this article the author discusses the latest developments in SCR controlled glass melting furnace boost systems.

Author
R Meuleman
Origin
Invenseys, The Netherlands
Journal Title
Glass Worldwide Sept/Oct 2010 72-76