Effects Of Counterions On Crack Growth In Vitreous Silica

Crack growth studies on vitreous silica were conducted in aqueous solutions as a function of pH in the range 1-14.

Author
G S White Et Al
Origin
National Bureau Of Standards
Journal Title
J Amer Ceram Soc 1987 70 12 891-895