Effects Of Batch Compositions On The Redox States Of Antimony In Tv-Glass Melts

To elucidate the effects of batch compositions on the redox states of antimony in TV-glass melts, the partial pressure of oxygen in the glass melts is measured by oxygen sensor which constitution is Pt//glass melt//Pt/Air/Zr02. As the temperature increases, the increasing p02 in the glass melt is observed due to the release of oxygen accompanied by the reduction of Sb5+ to Sb3+. The addition of sodium nitrate in the batch or increase in batch/cullet ratio helps to keep the glass melts more oxidizing state due to increasing pentavalent antimony concentration, which results in increasing p02 in the glass melts.

Author
M Yamamoto Et Al
Origin
Asahi Research Centre, Japan
Journal Title
Asahi Research Reports 50 2000 25-31
Sector
Special Glass
Class
S 2095

Request article (free for British Glass members)

Effects Of Batch Compositions On The Redox States Of Antimony In Tv-Glass Melts
Asahi Research Reports 50 2000 25-31
S 2095
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.