Effects Of Acid/Alkaline Strength, Temperature And Y-Irradiation On The Durability Of Fibreglass

Corrosion of fibreglass in aqueous solutions of different concentrations of H2SO4 or NaOH for different intervals of time was studied at room temperature and at 50 deg C. The effect of irradiating glass samples with 1, 3 and 7 Mrad (using 60Co as a source for y-rays) on the corrosion rate was also investigated. Results showed that fibreglass corrosion was higher in the acid than in alkaline solutions. Corrosion increased at higher temperature, with y-irradiation augmenting the observed corrosion of the glass in both acidic and alkaline solutions.

Author
N A El-Alaily & L S Ahmed
Origin
Nat Centre Radiation Research & Tech, Egypt
Journal Title
Glass Technol 43 2 2002 80-88
Sector
Glass Fibre
Class
GF 321

Request article (free for British Glass members)

Effects Of Acid/Alkaline Strength, Temperature And Y-Irradiation On The Durability Of Fibreglass
Glass Technol 43 2 2002 80-88
GF 321
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.