Effect Of Zno On The Crystallization, Microstructure, And Properties Of Glass-Ceramics In The Si02-Li20-Zn0-K20-P205 System

Six glasses in the Si02-Li20-Zn0-K20-P205 system were prepared. Starting from a dental glass-ceramic model composition, the Zn0 content was varied from 0.0 to 8.3 mol% with the molar ratios of the other components being invariant. Crystallisation processes of these glasses were investigated using high-temperature X-ray diffraction and differential scanning calorimetry.

Author
S Cramer Von Clausbruch Et Al
Origin
Ivoclar Ag, Germany
Journal Title
Glastech Ber Glass Sci Technol 74 8 2001 223-229
Sector
Special Glass
Class
S 2331

Request article (free for British Glass members)

Effect Of Zno On The Crystallization, Microstructure, And Properties Of Glass-Ceramics In The Si02-Li20-Zn0-K20-P205 System
Glastech Ber Glass Sci Technol 74 8 2001 223-229
S 2331
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.