Effect Of Water Concentration On The Properties Of Commercial Soda-Lime-Silica Glasses

The effect of water concentration on the properties of three commercial soda-lime-silica glasses has been measured. Properties included transformation temperature, viscosity, thermal expansion, electrical conductivity and refractive index.

Author
J M Jewell, M S Spess, J E Shelby
Origin
Alfred University
Journal Title
J Am Ceram Soc 1990 73 1 132-135
Sector
General
Class
G 357

Request article (free for British Glass members)

Effect Of Water Concentration On The Properties Of Commercial Soda-Lime-Silica Glasses
J Am Ceram Soc 1990 73 1 132-135