Effect Of Thermal Neutrons On Vickers Microhardness Of Some Ternary Borate Glasses

This paper investigates the Vickers indentation of some alkali borate glasses before and after subjecting to thermal neutron irradiation. The effect of load dependence of the microhardness values has also been investigated.