The Effect Of Thermal History On The Behaviour Of Heat Sensitive Glasses Containing Fluorine

A study of heat sensitive glasses has been carried out using compositions containing zinc and fluorine. The results indicate that when silica was substituted for ZnO the devitrification tendency of the glasses decreased independent of of the time in the furnace.

Author
V.V. Vargin
Origin
Unknown
Journal Title
Glass And Ceramics 1969 26 (7-8) 473-476
Sector
Primary Papers
Class
PP 895