Effect Of Temperature And Salt Additions On The Viscosity Of Borosilicate Glass.

The glass investigated was of Pyrex-brand composition, namely, SiO2 80.40% B2O3 11.9, Na2O 5.11, As2O3 0.50, Al203 1.49 and MgO 0.51. The following salts were introduced into the batch UO2(NO3)26H2O, Th(NO3)412H2O, (NH4OH) H2O7Mo03, BeCO, Ce(CO)35H2O, AND Na2SiF6.

Author
P.E. Frank And O.N Spiridonova
Origin
Unknown
Journal Title
Jour. Opt. Mech. Ind. [U.S.S.R], 9, 6 (1934)
Sector
Primary Papers
Class
PP 816