Effect Of Sucrose On Fabrication Of Ceramic Foams From Aqueous Slurries

Ceramic foams with porosity exceeding 90% were prepared by direct foaming and casting of aqueous suspensions containing cetyl trimethyl ammonium bromide (CTAB) as a foaming agent. Foaming of the suspensions, particularly with lower viscosity, was initially non-homogeneous but the foam appeared to homogenize with milling time. Addition of sucrose to ceramic suspensions resulted in lowering of the suspension viscosity, stabilized the foams by reducing drainage of the suspension, and minimized coalescence of bubbles leading to lower cell sizes in sintered foams. Ceramic foams prepared from sucrose based suspensions were strengthened to such an extent that foams with porosity above 90% could be machined in the green state.

Author
M Pradhan & P Bhargava
Origin
Indian Inst Technology, Kharagpur
Journal Title
J Am Ceram Soc 88 1 2005 216-218
Sector
Glass Ceramics
Class
GC 623

Request article (free for British Glass members)

Effect Of Sucrose On Fabrication Of Ceramic Foams From Aqueous Slurries
J Am Ceram Soc 88 1 2005 216-218
GC 623
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
19 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.