Effect Of Subsitution Of Li20 For Na20 On Surface Reactivity And Cellular Properties Of 45S5 Bioglass

There are reports that confirm the increasing effect of orally administered lithium on bone density. In this study, different concentrations of Li2O was substituted for Na2O in 45S5 bioglass and effect of these substitutions on both in vitro apatite formation ability and osteoblasts responses was studied.