Effect Of Small Glass Composition Changes On Flue Gas Emissions Of Glass Furnaces

Small changes in glass composition may have drastic consequences on evaporation rates of volatile glass components in glass melting furnaces. Transpiration evaporation tests have been applied to measure the impact of minor glass composition changes on evaporation rates of volatile glass components in simulated furnace atmospheres. Results of these evaporation tests were used to develop & optimise a universally applicable evaporation model to estimate evaporation rates & dust emissions for industrial glass melt furnaces. Mass transfer relations for the transport of volatile glass melt species into the turbulent gas phase were used to upscale the evaporation models valid for the lab tests to applications for industrial glass furnaces. In this paper, the impact of sulfur & chlorides on evaporation rates of sodium & potassium from multi-component silicate melts for industrial glass production will be demonstrated.

Author
H Van Limpt Et Al
Origin
Tno Glass Group, Netherlands
Journal Title
Verre 15 6 December/09 37-41
Sector
General
Class
G 3699

Request article (free for British Glass members)

Effect Of Small Glass Composition Changes On Flue Gas Emissions Of Glass Furnaces
Verre 15 6 December/09 37-41
G 3699
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.