Effect Of Silane Treatment On The Pore Structure Of Porous Glasses

Different kinds of controlled pore glasses (CPG) were modified with y-aminopropyltriethoxysilane (APS) in toluene or water solution. Their porous characteristics were changed as a result of this silane treatment in different ways, depending on the initial pore structure of the glasses. The results obtained clearly showd that APS deposition from toluene led to the formation of an aminopropylsiloxane multilayer on the surface of the CPG, whereas when deposited from its water solution a monolayer coverage was obtained.

Author
Z Foltynowicz Et Al
Origin
Mickiewicz University, Poland
Journal Title
Glass Technology 34 5 1993 206-209
Sector
Special Glass
Class
S 759

Request article (free for British Glass members)

Effect Of Silane Treatment On The Pore Structure Of Porous Glasses
Glass Technology 34 5 1993 206-209
S 759
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
14 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.