Effect Of Ribbon Orientation On The Fracture Toughness Of A Metallic-Glass-Ribbon-Reinforced Glass-Ceramic Matrix Composite

A commercially available amorphous metal ribbon incorporated into a glass-ceramic matrix has been assessed from the standpoint of fracture toughness.