Effect Of Process Vatiations On Anticancerous Drug Intercalation In Ceramic Based Delivery System

Two methods have been attempted to intercalate an anionic anti cancerous drug methotrextate (MTX) into Mg-Al layered double hydroxide (LDH): a) anion exchange method (sample A) and b) in situ co precipitation method followed by a soft hydrothermal treatment to form a biohybrid material. Both the materials obtained were characterised by powdered sample XRD, Fourier transformation infrared spectra , thermogravimetric-differential thermal analysis, particle size distribution analysis and field emission scanning electron microscopy.

Author
M Chakraborty Et Al
Origin
Cgcri, India
Journal Title
Trans Ind Ceram Soc 69 4 2010 229-234
Sector
Special Glass
Class
S 3686

Request article (free for British Glass members)

Effect Of Process Vatiations On Anticancerous Drug Intercalation In Ceramic Based Delivery System
Trans Ind Ceram Soc 69 4 2010 229-234
S 3686
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.