Effect Of Polymer Coatings On The Strength And Fatigue Behaviour Of Indented Soda-Lime Glass

All the coatings studied limited the access of water to the glass surface, thereby increasing the short term fatigue strength in water. The epoxy coating was the most effective in terms of both fatigue and ageing.