Effect Of Oxy-Fuel Conversion On Hydroxyl Content And Viscosity Of Glasses

Conversion of glass melting tanks to 100% oxy-fuel firing reduces NOx and particulate emissions, provides more efficient combustion, eliminates the need for heat recovery systems, and potentially increases product quality.