Effect Of Oxidation Of Mechanical Properties Of Fibrous Monolith Si3N4/Bn At Elevated Temperatures In Air

The oxidation behaviour and its effect on the mechanical properties of fibrous monolith Si3N4/BN after exposure to air at temperatures ranging from 1000-1400 deg C for up to 20h were investigated. After exposure at 1000C, only the BN cell boundary was oxidised, forming a B203 liquid phase. with increasing exposure temperature, the Si3N4 cells began to oxidise, forming crystalline Y2Si207, Si02, and silicate glass. However, in this case a weight loss was observed due to extensive vaporisation of the B203 liquid. After exposure at 1400 deg C, large YsSi207 crystals with a glassy phase formed near the BN cell boundaries. The oxidation behaviour significantly affected the mechanical properties of the fibrous monolith. The flexural strength and work-of-fracture decreased with increasing exposure temperature, while the noncatastrophic failure was maintained.

Author
Y Koh Et Al
Origin
Seoul Nat University, Korea
Journal Title
J Am Ceram Soc 85 12 2002 3123-3125
Sector
Glass Fibre
Class
GF 341

Request article (free for British Glass members)

Effect Of Oxidation Of Mechanical Properties Of Fibrous Monolith Si3N4/Bn At Elevated Temperatures In Air
J Am Ceram Soc 85 12 2002 3123-3125
GF 341
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
13 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.