Effect Of Nucleation On The Crystallisation And Dielectric Properties Of Strontium Titanate Glass-Ceramics

Differences in crystallisation behaviour and dielectric properties caused by heat treatment at 700 degreesC were attributed to a nucleation phenomenon.