Effect Of The Nature Of Crystallization On The Structure Of Foam Glass

The formation of homogeneous crystalline microstructure does not prevent the preparation of foam glass with homogeneous fine closed pores. comparitively large nonhomogeneous crystals impair the formability and even prevent the preparation of foam glass.