Effect Of Microwave Sintering On Structural, Ferroelectric, Dielecric And Mechanical Properties Of Sm-Doped Srbi4Ti4O15 Ceramics

Samarium substained SrBi4Ti4O15 (SBTi) ceramic, SrBi4-xSmxTi4O15 (SBSmTi) samples were prepared by solid. state reaction and processed using microwave sintering and conventional sintering techniques. Their morphological, dielectric, ferroelectric and mechanical properties were investigated. The microwave sintered samples shows high densities, 95% of the theoretical density were achieved with very short thermal treatments and with less soaking time. Relatively small plate-like grains were formed, and microstructure seemed not to be affected by doping or soaking time. The dielectric properties were measured as a function of frequency at 1MHz. The dielectric constant and loss tangent of the conventional and microwave sintered samples have ranged between (100-130) & (0.04 - 0.07) and (110-150) & (0.03-0.05) respectively. Compared with undoped SBTi, The incorporation of Sm3+ results in clear improvement for SBSmTi (x=0.75) on the dielectric properties ferroelectric and mechanical properties with increasing samarium content.

Author
A Rambabu & K C Raju
Origin
University Of Hyderabad, India
Journal Title
Journal Of The Australian Ceramic Society 48 1 2012 102-107
Sector
Special Glass
Class
S 3864

Request article (free for British Glass members)

Effect Of Microwave Sintering On Structural, Ferroelectric, Dielecric And Mechanical Properties Of Sm-Doped Srbi4Ti4O15 Ceramics
Journal Of The Australian Ceramic Society 48 1 2012 102-107
S 3864
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.