Effect Of Microstructure On The Properties Of Synthetic Refractory Aggregates

Four types of refractory aggregates (three sintered mullites using different starting materials and one tabular alumina) were synthesized by reaction sintering process and their properties evaluated. The microstructures of the aggregates have been studied by Scanning Electron Microscopy and correlated with the properties of the corresponding aggregates. The performance of these aggregates was also studied at high temperatures by using it in castables.

Author
S Kumar Et Al
Origin
National Metallurgical Labs, Jamshedpur, India
Journal Title
Trans Indian Ceram Soc 58 4 July-Aug 1999 89-91
Sector
Refractories
Class
R 359

Request article (free for British Glass members)

Effect Of Microstructure On The Properties Of Synthetic Refractory Aggregates
Trans Indian Ceram Soc 58 4 July-Aug 1999 89-91
R 359
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.