Effect Of The Lubricating Liuqid On The Glass-Cutting Process

Samples of 5mm float glass were used in a study of the effect of surface active materials on the glass-cutting process. A variety of lubricants was included and recommendations for specific applications are made.

Author
E I Ovchinnokova, V A Litvinov, And T A Khazova
Origin
Unknown
Journal Title
Glass And Ceramics 44 1-2 January-February 1987 48-51