Effect Of Lsgm Addition On Electrical Characteristics Of 8Ysz Ceramics For Solid Electrolyte

Effect of LSGM addition on electrical characteristics of 8YSZ ceramics has been studied. It was carried out to develop a solid electrolyte applicable for solid oxide fuel cell.