Effect Of Impact Angle And Velocity On The Fragment Size Distribution Of Glass Spheres

In this paper, the effects of impacted angle and impact velocity on the size distribution of glass fragments obtained in single particle impact experiments are investigated. This study suggests that the critical impact velocity required to initiate Hertzian crack in glass spheres under dynamic impact can be reasonably estimated based on slow compression test data. As the fragment size distribution can be characterised using a two-parameter Weibull equation, a simple approach is proposed to predict the fragment size distribution for glass particles filled under different impact arrangement based on the Weibull parameters.

Author
Y S Cheong Et Al
Origin
University Of Sheffield, Uk
Journal Title
Powder Technology 138 2003 189-200
Sector
General
Class
G 2901

Request article (free for British Glass members)

Effect Of Impact Angle And Velocity On The Fragment Size Distribution Of Glass Spheres
Powder Technology 138 2003 189-200
G 2901
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
16 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.