Effect Of Heat Treatment On Rapidly Quenched Agi-Based Silver Orthoborate Glasses Containing Large Amounts Of Agi

The effect of heat treatment on the twin-roller rapidly quenched 75AgI.18.7Ag20.6B203 glass was investigated by differential scanning calorimetry (DSC), high temperature X-ray diffraction (XRD), and field-emission-type scanning electron microscopy.

Author
N Itakura Et Al
Origin
Osaka Prefecture University, Japan
Journal Title
J Am Ceram Soc 80 12 1997 3209-3212