Effect Of Grinding And Polishing On The Results Of Analyses Of Glass By The Electron Probe. (In Czech)

A study has been made of the possible effect of sample preparation in aqueous media on electron probe investigations. The results indicate that in the case of glasses with poor chemical durability contact with water should be avoided during treatment and higher accelerating voltages should be selected.