Effect Of Glass Additions On The Indentation-Strength Behaviour Of Alumina

The effect of small calcium aluminosilicate (CAS) glass additions on the microstructure and the flaw tolerance of alumina ceramics is investigated, and the results compared to a high-purity alumina. The high-purity alumina specimens were dense with microstructures consisting of a uniform grain size distribution and equiaxed grain morphology. Additions of only 1wt% glass phase resulted in a bimodal grain size distribution containing large, elongated grains within a fine-grain matrix.

Author
H L O'Donnell Et Al
Origin
Carnegie Mellon University, Usa
Journal Title
J Am Ceram Soc 78 4 1995 849-856
Sector
Special Glass
Class
S 855

Request article (free for British Glass members)

Effect Of Glass Additions On The Indentation-Strength Behaviour Of Alumina
J Am Ceram Soc 78 4 1995 849-856
S 855
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 9 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.