Effect Of Fluorine On The Optical Properties Of Baf2-Bao-La2O3-B2O3 Glasses Prepared By Containerless Processing

The glass-forming region of the BaO-La2O3-B2O3 ternary system was determined by using a conainerless processing. The glass transition temperature, density, refractive index and Abbe number were investigated. The efects of the substitution of fluorine for oxygen on the refractive index and Abbe number were discussed on the basis of electronic polarizability and resonance wavelength of oscillator.

Author
J Chung Et Al
Origin
University Of Tokyo, Japan
Journal Title
Int J Applied Glass Science 10 2019 181-189
Sector
Special Glass
Class
S 4520

Request article (free for British Glass members)

Effect Of Fluorine On The Optical Properties Of Baf2-Bao-La2O3-B2O3 Glasses Prepared By Containerless Processing
Int J Applied Glass Science 10 2019 181-189
S 4520
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 11 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.