Effect Of Fiberization Process On Glass Fibre Surfaces

Surface properties such as chemical durability are of critical importance to the behaviour & performance of fine diameter, discontinuous glass fibre. In addition to bulk composition, these properties are infuenced by the method of fiberization & the specific process variables employed in production. Controlled dissolution studies combined with SEM & surface chemical analysis were used to evaluate process effects, particularly as they relate to durability & persistence of fibres in the lung. Results indicated that fibres produced by pure flame attenuation exhibited a unique concentric structure with an outer surface that can be more durable than the bulk composition would indicate. Fibres produced by air attenuation in either continous draw or rotary processes are more uniform with surfaces that are more open and reactive to moisture or simulated body fluids.

Author
J F Bauer
Origin
Johns Manville Tech Centre, Usa
Journal Title
Ceramic Trans 82 1998 187-202
Sector
Glass Fibre
Class
GF 215

Request article (free for British Glass members)

Effect Of Fiberization Process On Glass Fibre Surfaces
Ceramic Trans 82 1998 187-202
GF 215
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
15 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.