Effect Of Deposition Conditions On Physical Properties Of Sputtered Silicon Oxynitride Thin Films On Float Glass

Silicon oxynitride layers have been widely used to tailor the optical performance and mechanical resistance of multilayer optical coatings. The key issue for their reliable large-scale application on a glass substrate is the effect of technological parameters on their performance. This article reports on the interrelationship between the conditions of the reactive magnetron deposition process and composition, structure and in turn optical and mechanical properties.

Author
L Simurka Et Al
Origin
Sisecam, Turkey
Journal Title
Int J Appl Glass Sci 9 2018 403-412
Sector
Flat glass
Class
F 4087

Request article (free for British Glass members)

Effect Of Deposition Conditions On Physical Properties Of Sputtered Silicon Oxynitride Thin Films On Float Glass
Int J Appl Glass Sci 9 2018 403-412
F 4087
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 9 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.