Effect Of Crystallization On Thermal Conductivity And Specific Heat Of Two Corning Glass-Ceramics

A magnesium aluminosilicate glass-ceramic has been heat-treated at 900, 1010, 1200 and 1260 degres C for up to 90 minutes, and the effect on the thermal conductivity between 30 and 300K has been studied.