Effect Of Crystallisation Temperature On Electrical Properties Of Er3+/Yb3+-Sro.Tio2 Borosilicate Glass

Er3+/Yb3+ doped 22[3SrO.2TiO2].30 [2sIo2.B2O3] glass and glass-ceramics are developed and investigated for their electrical properties. The degree of crystallization is varied by means of crystallisation temperature ranging from 600-1000 deg C. In glass-ceramic samples, two major crystalline phases, Sr3Ti2O7 and TiO2, are confirmed by diffraction analysis. The best crystallized glass-ceramic sample shows 100-1 50 times lower impedance in temperature range, 200-300 deg C, than the uncrystallized glass. Electrical relaxation corresponding tot he crystalline phase can be isolated in frequency domain.

Author
A Maheshwari, Et Al
Origin
Banaras Hindu University, Varanasi, India
Journal Title
Int J Appl Glass Sci 7 3 Sept/2016 319-327
Sector
Glass Ceramics
Class
GC 882

Request article (free for British Glass members)

Effect Of Crystallisation Temperature On Electrical Properties Of Er3+/Yb3+-Sro.Tio2 Borosilicate Glass
Int J Appl Glass Sci 7 3 Sept/2016 319-327
GC 882
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
12 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.