Effect Of Cr203, Zr02 And Lif On Nucleation And Crystallization Of Nepheline Syenite-Dolomite Glass-Ceramic Compositions

Inexpensive nepheline-pyroxene glass-ceramics of superior mechanical, and thermal properties could be easily prepared from nepheline syenite and dolomite rock mixture by using the conventional glass preparation and heat treatment methods.

Author
A W El-Shennawi Et Al
Origin
National Research Centre, Cairo, Egypt
Journal Title
Glastech Ber Glass Sci Technol 74 11/12 2001 317-323
Sector
Glass Ceramics
Class
GC 443