The Effect Of Cation Size On The Electrical Relaxations Of Glassy And Molten Ca(No3)2-4.1H2O Mixtures

The dielectric permittivity and loss of 0.6(Ca(NO3)2-4.1H2O)-0.4MNO3, where M = K or Li, have been measured from 77K to a temperature above their glass transitions over a frequency range from 12 Hz to 100 kHz.

Author
S K Jain, K Pathmanathan, G P Johari
Origin
Mcmaster University
Journal Title
Phys Chem Glasses 1988 29 5 198-203
Sector
Special Glass
Class
S 180

Request article (free for British Glass members)

The Effect Of Cation Size On The Electrical Relaxations Of Glassy And Molten Ca(No3)2-4.1H2O Mixtures
Phys Chem Glasses 1988 29 5 198-203
S 180