Effect Of Aqueous-Based Mechanical Polishing On The Nanoindentation Response Of Borosilicate Glasses

In this study, it is shown that the act of polishing certain borosilicate glass compositions in an aqueous environment directly affects the nanomechanical response to several micrometers, reducing the measured elastic modulus and hardness by ~20% and ~35% respectively.

Author
B L Hackett Et Al
Origin
University Tennessee, Knoxville, Usa
Journal Title
Applied Glass Science 10 3 July 2019 302-306
Sector
Special Glass
Class
S 4525

Request article (free for British Glass members)

Effect Of Aqueous-Based Mechanical Polishing On The Nanoindentation Response Of Borosilicate Glasses
Applied Glass Science 10 3 July 2019 302-306
S 4525