The Effect Of Amber Cullet Additions On Amber Glass Transmission

Results of experimental melts indicate that additions of amber cullet to a glass of similar composition cause the 550 nm transmission of the final glass to increase by approx. 0.15% for every percent addition of amber cullet above 10% total cullet.