Effect Of Alkali Cations On The Compressibility Of Maisi308 Glasses (M=Na, K, Rb, Cs) In The Pressure Range Up To 6.0 Gpa

The refractive indices of RbAlSi3O8 and CsAlSi3O8 glasses in the range of pressures up to 6.0 GPa were measured using a polarisation-interference microscope and a diamond anvil apparatus. The changes in the relative density which characterise the compressibility of the glasses were estimated in the pressure range under investigation from the measured refractive indices within the framework of the theory of photoelasticity. Although the molar contents of Al2O3 and M2O are identical in the MAlSi3O8 glasses (M=Na, K, Rb, Cs), the isothermal initial bulk modulus (Kt,o) of these glasses decreases in the order Na+, K+, Rb+, and practically does not change when Rb+ is replaced by Cs+. This change in Kt,o indicates an increase in the degree of polymerisation of the structural network of the glasses containing Rb+ or Cs+. The increase in Kt for glasses in teh series of alkali metal cations can be explained by teh fact that the voids are occupied by cations K+, Rb+, Cs+, which have a larger orbital radius than Na+, and more strongly inhibit compression.

Author
R G Kuryaeva
Origin
Russian Academy Sciences
Journal Title
Phys Chem Glasses 53 4 2012 151-157
Sector
Special Glass
Class
S 3942

Request article (free for British Glass members)

Effect Of Alkali Cations On The Compressibility Of Maisi308 Glasses (M=Na, K, Rb, Cs) In The Pressure Range Up To 6.0 Gpa
Phys Chem Glasses 53 4 2012 151-157
S 3942
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 12 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.