Early-Stage Microstructure Development In Bi-Sr-Ca-Cu-O Glasses

Amorphous samples of Bi2Sr2Ca1Cu2Ox were produced by quenching from the melt. The early-stage microstructure development in these samples was monitored using XRD, DTA, and hot-stage TEM. It was observed that the molten glass undergoes phase separation during initial quenching and that subsequent refinement of these features generates the initial DTA exotherm during heating.

Author
S Kim Et Al
Origin
University Of Arizona, Usa
Journal Title
J Am Ceram Soc 76 12 1993 3087-3092
Sector
Special Glass
Class
S 791